[article]
Titre : |
Internal oxidation of Fe–3%Si alloys annealed under H2O–H2 atmosphere |
Type de document : |
texte imprimé |
Auteurs : |
S. Yamazaki, Auteur ; F. Takahashi, Auteur ; T. Kubota, Auteur |
Année de publication : |
2011 |
Article en page(s) : |
pp. 476–480 |
Note générale : |
Génie Mécanique |
Langues : |
Anglais (eng) |
Mots-clés : |
Internal oxidation Oxygen diffusion Precipitate morphology Silicon steel |
Index. décimale : |
620.1 Essais des matériaux. Défauts des matériaux. Protection des matériaux |
Résumé : |
Internal oxidation phenomena during decarburization annealing are very important in the manufacturing process of grain oriented electrical steel. In the present study, the internal oxidation of nearly pure Fe–3%Si alloy was investigated, as a basic study for decarburization annealing. Annealing was performed at various equation image ratios and at 1123 K for 300 s. The transition of external to internal oxidation took place at equation image around 0.01. The morphologies of oxide in the internal oxidation zone (IOZ) were filamentary or needle-like shapes and different from the reported oxide shapes in industrial electrical steel. These peculiar morphologies affected the kinetic aspects such as the depth and the enrichment of oxide in the IOZ.
|
DEWEY : |
620.1 |
ISSN : |
0947-5117 |
En ligne : |
http://onlinelibrary.wiley.com/doi/10.1002/maco.201005862/abstract |
in Materials and corrosion > Vol. 62 N° 6 (Juin 2011) . - pp. 476–480
[article] Internal oxidation of Fe–3%Si alloys annealed under H2O–H2 atmosphere [texte imprimé] / S. Yamazaki, Auteur ; F. Takahashi, Auteur ; T. Kubota, Auteur . - 2011 . - pp. 476–480. Génie Mécanique Langues : Anglais ( eng) in Materials and corrosion > Vol. 62 N° 6 (Juin 2011) . - pp. 476–480
Mots-clés : |
Internal oxidation Oxygen diffusion Precipitate morphology Silicon steel |
Index. décimale : |
620.1 Essais des matériaux. Défauts des matériaux. Protection des matériaux |
Résumé : |
Internal oxidation phenomena during decarburization annealing are very important in the manufacturing process of grain oriented electrical steel. In the present study, the internal oxidation of nearly pure Fe–3%Si alloy was investigated, as a basic study for decarburization annealing. Annealing was performed at various equation image ratios and at 1123 K for 300 s. The transition of external to internal oxidation took place at equation image around 0.01. The morphologies of oxide in the internal oxidation zone (IOZ) were filamentary or needle-like shapes and different from the reported oxide shapes in industrial electrical steel. These peculiar morphologies affected the kinetic aspects such as the depth and the enrichment of oxide in the IOZ.
|