[article]
Titre : |
Metallic interconnects for solid oxide fuel cell: Performance of reactive element oxide coating during long time exposure |
Type de document : |
texte imprimé |
Auteurs : |
S. Fontana, Auteur ; S. Chevalier, Auteur ; G. Caboche, Auteur |
Année de publication : |
2011 |
Article en page(s) : |
pp. 650–658 |
Note générale : |
Génie Mécanique |
Langues : |
Anglais (eng) |
Mots-clés : |
Metallic interconnect MOCVD Reactive element SOFC |
Index. décimale : |
620.1 Essais des matériaux. Défauts des matériaux. Protection des matériaux |
Résumé : |
One of challenges in improving the performance and cost-effectiveness of SOFCs (solid oxide fuel cells) is the development of suitable interconnects materials. Chromia-forming alloys and especially ferritic stainless steels, like Crofer22APU, are considered to be among the most promising candidate materials as interconnects in SOFC stacks. However, the performance of chromia-forming materials can be limited by the low electronic conductivity of the oxide scale (high ASR – area specific resistance – value). Such degradation are unacceptable regarding the long-term operation (>40 000 h). A previous study 1 demonstrated that in air, the addition of a nanometric reactive element oxide (La2O3) layer applied by metal organic chemical vapor deposition (MOCVD) drastically improved both corrosion rate and electrical properties of Crofer22APU and Haynes230 alloys for 100 h at 800 °C. In this present study coating performances were checked after 10 months (7500 h) and 20 months (15 000 h) at 800 °C in air. The corrosion products were carefully analyzed by SEM, EDX, and XRD. ASR measurements are realized after long time exposure. This study demonstrates that the Crofer22APU alloy has a good oxidation resistance after 15 000 h in air but this alloy has an ASR value equal to 0.370 Ω cm2. The coatings composed of a thin reactive element oxide such as La2O3 resulted in an important improvement in the high temperature oxidation resistance; the ASR values are equal to 0.154 Ω cm2. Haynes230 alloy has a better oxidation resistance but the formation of an insulating Al2O3/SiO2 layer could be detrimental.
|
DEWEY : |
620.1 |
ISSN : |
0947-5117 |
En ligne : |
http://onlinelibrary.wiley.com/doi/10.1002/maco.201005857/abstract |
in Materials and corrosion > Vol. 62 N° 7 (Juillet 2011) . - pp. 650–658
[article] Metallic interconnects for solid oxide fuel cell: Performance of reactive element oxide coating during long time exposure [texte imprimé] / S. Fontana, Auteur ; S. Chevalier, Auteur ; G. Caboche, Auteur . - 2011 . - pp. 650–658. Génie Mécanique Langues : Anglais ( eng) in Materials and corrosion > Vol. 62 N° 7 (Juillet 2011) . - pp. 650–658
Mots-clés : |
Metallic interconnect MOCVD Reactive element SOFC |
Index. décimale : |
620.1 Essais des matériaux. Défauts des matériaux. Protection des matériaux |
Résumé : |
One of challenges in improving the performance and cost-effectiveness of SOFCs (solid oxide fuel cells) is the development of suitable interconnects materials. Chromia-forming alloys and especially ferritic stainless steels, like Crofer22APU, are considered to be among the most promising candidate materials as interconnects in SOFC stacks. However, the performance of chromia-forming materials can be limited by the low electronic conductivity of the oxide scale (high ASR – area specific resistance – value). Such degradation are unacceptable regarding the long-term operation (>40 000 h). A previous study 1 demonstrated that in air, the addition of a nanometric reactive element oxide (La2O3) layer applied by metal organic chemical vapor deposition (MOCVD) drastically improved both corrosion rate and electrical properties of Crofer22APU and Haynes230 alloys for 100 h at 800 °C. In this present study coating performances were checked after 10 months (7500 h) and 20 months (15 000 h) at 800 °C in air. The corrosion products were carefully analyzed by SEM, EDX, and XRD. ASR measurements are realized after long time exposure. This study demonstrates that the Crofer22APU alloy has a good oxidation resistance after 15 000 h in air but this alloy has an ASR value equal to 0.370 Ω cm2. The coatings composed of a thin reactive element oxide such as La2O3 resulted in an important improvement in the high temperature oxidation resistance; the ASR values are equal to 0.154 Ω cm2. Haynes230 alloy has a better oxidation resistance but the formation of an insulating Al2O3/SiO2 layer could be detrimental.
|